DVD-87: Innerlayer Handling Series, Part 7: Lamination

Member: $236.00

Nonmember: $315.00

Free Review

Seventh and final video in the Innerlayer Handling Series details pin registration lay-up and lamination processes, and explains the step-by-step sequence of laying up a typical multilayer panel. Proper handling of caul plates, separator plates, copper foil, prepreg sheets and innerlayers is described. The lamination section examines three different types of vacuum press systems: vacuum enclosed presses, vacuum frames and turkey bag systems. Also contains a description of the process for mass lamination and a brief discussion of automatic optical inspection (AOI) and surface treatment operations. Time: 28 minutes.

More about the DVD-R Format used for this product.

Product ID: 87-MT-0-DVD-0-EN-0