IPC-SM-817A: General Requirements for Dielectric Surface Mount Adhesives

Member: $41.00

Nonmember: $83.00

Provides requirements for dielectric adhesives to hold components in place from the mounting to the soldering process and identifies test methods to ensure their long term properties. 9 pages. Released December 2014.