4104: Specification for High Density Interconnect (HDI) and Microvia Materials

Member: $66.00

Nonmember: $131.00

Covers the various conductive and dielectric materials that can be used for the fabrication of HDI and microvias. The 23 specification sheets included in IPC/JPCA-4104 cover the qualification and conformance requirements for such materials as photoimageable dielectric dry films and liquids, epoxy blends and coated foils. IPC/JPCA-4104 also includes six new test methods developed specifically for the testing of HDI and microvia materials. 92 pages. Released May 1999.