DVD-38: Liquid Photo-Imageable Solder Mask

Member: $205.00

Nonmember: $257.00

Free Review

Begins by explaining the purpose and advantages of liquid photo-imageable solder mask. Visually examines each step in the application process, including surface preparation (both abrasive and chemical pre-wash), screen and curtain coating (including thickness evaluation), tack drying, exposure (including environmental controls, clothing, artwork alignment, and machine operation /maintenance), developing (including machine operation for both aqueous and solvent systems), inspection for typical defects, and the operation of a typical curing oven. (Winner of the Vision and Telly Awards.) Time: 29 minutes.

More about the DVD-R Format used for this product.

Product ID: 38-MT-0-DVD-0-EN-0