IPC-4562A-WAM1: Metal Foil for Printed Board Applications
IPC-4562A-WAM1 covers metal foils supported by carrier films and unsupported foils suitable for subsequent use in printed boards. The Amendment 1 that has been inserted into the base document added back the light cold rolled-wrought copper foil (/6 [Cu-W6] that was previously removed during the revision A actions. Unless otherwise agreed upon between the user and supplier (AABUS), metal foils shall be considered acceptable, so long as the requirements in this specification are met.31 pages. Released January 2016.
Number of Pages: 31
ISBN: 978-1-61193-232-4
Product ID: 4562-STD-0-D-W1-EN-A