IPC-7530A: 群焊工艺温度曲线指南(再流焊和波峰焊

Member: $84.00

Nonmember: $168.00

本标准的目的是为开发温度曲线提供有效和实用的信息,以生产可接受的锡铅和无铅的电子组件。该修订版将原来标准的重点从再流温度曲线扩展到包括激光焊曲线、选择焊曲线、波峰焊曲线或其他焊接曲线。该修订版还包括一个全彩色故障排除指南,用于解决可归因于分析的常见缺陷。

Single-Device DRM-Protected Document

This document has single-device/user digital rights management (DRM) protection. This document will only be accessible by a single user on a single device. If you are purchasing this DRM-protected document for another user, you will need to provide contact information for that user when placing your order.