IPC-9121-AM2: Troubleshooting for Printed Board Fabrication Processes, Amendment 2

Member: $27.00

Nonmember: $53.00

The amendment 2 to IPC-9121 provides new troubleshooting topics on hole quality, laser drilling, microvias, drill smear, electroless nickel, organic solderability preservative (OSP) and rigid-flex boards.

Number of Pages: 36
ISBN: 978-1-61193-497-7
Product ID: 9121-STD-0-D-A2-EN-0