The IPC-9505 standard provides details of test methodologies for cleaning chemistry compatibility with electronic assembly materials that replace those in MIL-STD-202 Method 215 for testing electronic and electrical components such as capacitors, resistors, transformers and inductors. The test methods can also be used, when applicable, to parts not covererd by military specifications or drawings
Number of Pages: 52
Release Date: 10/12/2017
ISBN: 978-1-61193-318-5