IPC-TR-579: Round Robin Reliability Evaluation of Small Diameter Plated Through Holes in PWBs

Member: $66.00

Nonmember: $131.00

Approximately 200,000 plated through-holes, covering primarily electroplated but also electroless technology, were exposed to several different thermal cycles. A number of PTH diameters, board constructions and plating thicknesses were evaluated. 80 pages. Released September 1988.