IPC-WP-019: An Overview on Global Change in Ionic Cleanliness Requirements

Member: $42.00

Nonmember: $83.00

This document provides an overview of ionic cleanliness requirements, providing examples of tests and requirements for acceptability from a residue/cleanliness standpoint. The history of ROSE testing is also provided, with explanations of the shortcomings of that testing.

Number of Pages: 16