IPC/JEDEC-9703: IPC/JEDEC Mechanical Shock Test Guidelines for Solder Joint Reliability

Establishes mechanical drop and shock and test guidelines for assessing solder joint reliability of printed board assemblies from system to component level. This document addresses methods to define mechanical shock use-conditions, methods to define system level, system printed board level and component test board level testing that correlate to such use conditions and guidance on the use of experimental metrologies for mechanical shock tests. 42 pages. Released March 2009.

Included in the C-103 and C-1000 Collections.

Published Date
Pages
42
DoD Adopted
No
ANSI Approved
No