IPC-CC-830B-AM1: Qualification and Performance of Electrical Insulating Compound for Printed Wiring Assemblies

IPC-CC-830B prescribes qualification and performance requirements of conformal coatings. Amendment 1 provides updated requirements for moisture and insulation resistance and temperature and humidity aging and additional information on coating classifications.