IPC-8921: Requirements for Woven and Knitted Electronic Textiles (E-Textiles) Integrated with Conductive Fibers, Conductive Yarns and/or Wires

The IPC-8921 standard provides and defines industry test methods and guidance for providing performance data on key characteristics and durability of woven and knitted e-textiles integrated with conductive fibers, conductive yarns and/or wires.

The IPC-8921 standard also provides classicfications for woven and knitted e-textiles, fibers, yarns and wires and includes 20 new terms and defintions for e-textiles.