Current Revision
IPC-A-640A
IPC-A-640A: Acceptance Requirements for Optical Fiber, Optical Cable and Hybrid Wiring Harness Assemblies
The IPC-A-640A standard provides acceptance requirements and technical insight that have been removed from acceptance standards for cable and wire harness assemblies incorporating optical fiber, optical cable and hybrid wiring technology. The IPC-A-640A is intended for use by the design engineer, manufacturing engineer, quality engineer and other individuals responsible for tailoring specific requirements to the applicable performance class.
Published Date
ISBN
978-1-63816-058-8
Pages
104
DoD Adopted
No
ANSI Approved
No