Current Revision
IPC-J-STD-002E

EIA/IPC/JEDEC J-STD-002E: Solderability Tests for Component Leads, Terminations, Lugs, Terminals and Wires - English

IPC-J-STD-002E prescribes test methods, defect definitions, acceptance criteria, and illustrations for assessing the solderability of electronic component leads, terminations, solid wires, stranded wires, lugs, and tabs. The IPC-J-STD-002E standard also includes a test method for the resistance to dissolution/dewetting of metallization. IPC-J-STD-002E is intended for use by both supplier and user. The IPC-J-STD-002E standard was developed by the following three organizations: ECIA, IPC and JEDEC.

Published Date
ISBN
978-1-61193-337-6
Pages
65
DoD Adopted
No
ANSI Approved
No