J-STD-006B-JP: Requirements for Electronic Grade Solder Alloys and Fluxed and Non-Fluxed Solid Solders for Electronic Soldering Applications

This is the Japanese language version of J-STD-006B.

This standard prescribes the nomenclature, requirements and test methods for electronic grade solder alloys; for fluxed and non-fluxed bar, ribbon, and powder solders, for electronic soldering applications; and for ''special'' electronic grade solders. This is a quality control standard and is not intended to relate directly to the material's performance in the manufacturing process. Solders for applications other than electronics should be procured using ASTM B-32.

This standard is one of a set of three joint industry standards that prescribe the requirements and test methods for soldering materials for use in the electronics industry: IPC/EIA J-STD-004, Requirements for Soldering Fluxes; IPC/EIA J-STD-005, Requirements for Soldering Pastes; IPC J-STD-006, Requirements for Electronic Grade Solder Alloys and Fluxed and Non-Fluxed Solid Solders for Electronic Soldering Applications. 27 pages. Released January 2006.

Published Date
Pages
27
DoD Adopted
No
ANSI Approved
No