Lead-free electronics continues to be a concern of the aerospace, defense, and high performance products (ADHP) industries. This is primarily due to the lack of data and knowledge to: thoroughly categorize performance under harsh service conditions and provide a level of confidence in reliability assessments of Pb-free electronics equal to those for traditional tin-lead electronics. To help close...