Current Revision
IPC-4103B standard covers the requirements for clad and unclad plastic laminate and bonding layer materials to be used for the fabrication of printed boards for microstrip, stripline and high speed digital electrical and electronic circuits. In addition to better definitions of inclusions and how to properly classify them; redefine "substrates" as, "fabricated sheets"; and a more proper definition...