Close

IPC-4204 Amendment

Products

Document #:
Revision
A
Product Type
Released:  10/01/2013
Language
English
Metal-Clad Dielectrics for Use in Fabrication of Flexible Printed Circuitry Amendment 1 to IPC-4204A modifies the standard by replacing five sections in the document (sections: 1.1.2 Specific Designation; 2.1 IPC; 2.5 ISO; 3.5.2 Wrinkles, Creases, Streaks and Scratches; and 3.9 Electrical Requirements) to clarify the meanings of these sections.