The IPC J-STD-004C WAM1 standard prescribes general requirements for the classification and characterization of fluxes for high quality solder interconnections. The IPC J-STD-004C WAM1 standard may be used for quality control and procurement purposes. Soldering flux materials include the following: liquid flux, paste flux, solder paste, solder cream as well as flux-coated and flux-cored solder...

IPC-2231 - Revision A - Standard Only

DFX Guidelines

Document #:
Revision
A
Product Type
Released:  10/27/2021
Language
English
Current Revision
IPC-2231A provides guidelines for establishing a best practice methodology for use in developing a formal DFX (Design for Manufacturing, Fabrication, Assembly, Testability, Cost, Reliability, Environment, Reuse) process for layout of printed boards.
Document #:
Revision
B
Product Type
Released:  04/12/2022
Language
English
Current Revision
The IPC-9701B standard establishes a thermal cycling test method to characterize the fatigue lifetimes of surface mount solder attachments of electronic assemblies. The surface mount devices may be solder-attached to rigid, flexible or rigid-flex printed boards. The characterization results can be used to predict the field lifetime of solder attachments for the use environments and conditions of...
Document #:
Revision
A
Product Type
Released:  05/31/2022
Language
English
Current Revision
The IPC-A-640A standard provides acceptance requirements and technical insight that have been removed from acceptance standards for cable and wire harness assemblies incorporating optical fiber, optical cable and hybrid wiring technology. The IPC-A-640A is intended for use by the design engineer, manufacturing engineer, quality engineer and other individuals responsible for tailoring specific...
Document #:
Revision
B
Product Type
Released:  09/08/2016
Language
English
Current Revision
This document is the product of the IPC Electrochemical Migration (ECM) Task Group. It was drafted to provide guidance regarding implementation of the User Guide for the IPC-TM-650, Method 2.6.25, Conductive Anodic Filament (CAF) Resistance and Other Internal Electrochemical Migration Testing to evaluate the effects of mechanical stress, laminate material fracturing, ionic contamination, moisture...

IPC-SM-817 - Revision A - Standard Only

General Requirements for Dielectric Surface Mount Adhesives

Document #:
Revision
A
Product Type
Released:  12/23/2014
Language
English
Current Revision
Provides requirements for dielectric adhesives to hold components in place from the mounting to the soldering process and identifies test methods to ensure their long term properties. 9 pages. Released December 2014.
Document #:
Revision
A
Product Type
Released:  10/28/2022
Language
English
Current Revision
The IPC-9202A, Material and Process Characterization/Qualification Test Protocol that records changes in Surface Insulation Resistance (SIR) on a representative sample of a printed circuit assembly (PCA). It quantifies any deleterious effects that might arise from solder flux or other process residues left on external surfaces after soldering, which can cause unwanted electro-chemical reactions...
Document #:
Revision
C
Product Type
Released:  11/20/2020
Language
English
Current Revision
The IPC-2581C standard specifies the XML schema that represents the intelligent data file format used to describe printed board and printed board assembly products with details sufficient for tooling, manufacturing, assembly, and inspection requirements. This format may be used for transmitting information between a printed board designer and a manufacturing or assembly facility. The data is most...

IPC-1401 - Revision A - Standard Only

Corporate Social Responsibility Management System Standard

Document #:
Revision
A
Product Type
Released:  11/29/2021
Language
English
Current Revision
The IPC-1401A standard specifies the requirements and best practice guidelines for an effective corporate social responsibility (CSR) management system to help an enterprise integrate CSR as a customer requirement into products and value chain activities, as well as to identify and manage CSR risks and opportunities through cooperation with customers and suppliers, to enhance the competitive...

IPC/JEDEC-J-STD-035 - Revision A - Standard Only

Acoustic Microscopy for Nonhermetic Encapsulated Electronics Devices

Document #:
Revision
A
Product Type
Released:  02/16/2023
Language
English
Current Revision
IPC/JEDEC J-STD-035A test method defines the procedures for performing acoustic microscopy on nonhermetic encapsulated electronic devices. IPC/JEDEC J-STD-035A method provides users with an acoustic microscopy process flow for detecting anomalies (delaminations, cracks, mold compound voids, etc.) nondestructively in encapsulated electronic devices while achieving reproducibility

IPC-1720 - Revision A - Standard Only

Assembly Qualification Profile

Document #:
Revision
A
Product Type
Released:  08/02/2004
Language
English
Current Revision
Developed by the OEM council of the IPC, IPC-1720A categorizes electronic assembly manufacturer capabilities and supplies the OEM customer with detailed, substantive information. This program simplifies auditing processes and reduces the frequency of audits, thereby decreasing paperwork and improving efficiency. Company and Site Description, Site Capability Snap Shot, Equipment Profile (Pre-site...

IPC-9261 - Revision A - Standard Only

In-Process DPMO and Estimated Yield for PCAs

Document #:
Revision
A
Product Type
Released:  10/01/2006
Language
English
Current Revision
Now updated to align with IPC-7912A for end item DPMO, this document defines consistent methodologies for computation of in-process defects per million opportunities (DPMO) metrics for any evaluation stage in the assembly process. It is intended for use in measuring in-process assembly steps rather than end product determination. Calculation of completed item DPMO is addressed in IPC-7912A. A...

IPC-9201 - Revision A - Standard Only

Surface Insulation Resistance Handbook

Document #:
Revision
A
Product Type
Released:  09/19/2007
Language
English
Current Revision
Surface Insulation Resistance (SIR) testing is a tool used not only for characterization testing of production processes such as solder masks, soldering flux, and conformal coatings, but also for examining the electrochemical reactions at each stage of the electronic assembly production process. This handbook covers the terminology, theories, test procedures and test vehicles of SIR testing...

IPC-J-STD-003 - Revision C - Standard with Amendments 1 & 2

Solderability Tests for Printed Boards

Document #:
Revision
C
Released:  10/02/2017
Language
English
Current Revision
The IPC-J-STD-003C-WAM1&2 standard prescribes test methods, defect definitions and illustrations for assessing the solderability of printed board surface conductors, attachment lands and plated-through holes (PTHs). The IPC-J-STD-003C-WAM1&2 standard is not intended to verify the potential of successful processing at assembly or to evaluate design impact on wettability. The IPC-J-STD-003C-WAM1&2...

IPC-7912 - Revision A - Standard Only

End-Item DPMO for Printed Circuit Board Assemblies

Document #:
Revision
A
Product Type
Released:  01/01/2004
Language
English
Current Revision
Finally - an end to the confusion when calculating defect opportunities for benchmarking! For customers and manufacturers, it seems like every company has a unique way of calculating defects and then reporting on quality. In a complex electronics assembly operation, is it best to calculate using the number of components? The number of leads? What about solder joints? How can companies calculate...
Document #:
Revision
B
Product Type
Released:  11/01/2016
Language
English
Current Revision
This standard provides a marking and labeling system that aids in assembly, rework, repair and recycling and provides for the identification of: those assemblies that are assembled with lead-containing or lead-free solder; components that have lead-containing or lead-free second level interconnect terminal finishes and materials; the maximum component temperature not to be exceeded during assembly...
Document #:
Revision
A
Product Type
Released:  05/31/2022
Language
English
Current Revision
The IPC-D-620A standard is the cable and wiring harness, systems-level design requirements companion to IPC/WHMA-A-620 and its associated space addendum. The intent of IPC-D-620A is to set forth the general design requirements for electrical wiring harnesses and cable assemblies. The IPC-D-620A is intended for use by the design engineer, manufacturing engineer, quality engineer, or other...

IPC-PE-740 - Revision A - Standard Only

Troubleshooting for Printed Board Manufacture and Assembly

Document #:
Revision
A
Product Type
Released:  12/01/1997
Language
English
Current Revision
This is the document all process engineers must have! Useful for day-to-day problem solving, it contains case histories of problems and corrective action in the design, manufacture, assembly and testing of printed wiring products. Each section has been updated to reflect today's manufacturing challenges. Sections address documentation, phototooling, raw materials, mechanical operations, hole...
Document #:
Revision
A
Product Type
Released:  12/23/2014
Language
English
Current Revision
This document provides the designer/user with guideline information related to the use of pressure sensitive adhesives (PSAs) for fabrication and assembly of flexible, rigid or rigid-flex printed boards, membrane switches and component attachments. It also provides information on adhesive types available, their inherent strengths, weaknesses, limitations and correct processes needed for creating...

IPC-9850 - Revision A - Standard Only

Surface Mount Placement Equipment Characterization

Document #:
Revision
A
Product Type
Released:  12/21/2011
Language
English
Current Revision
This standard establishes the parameters, procedures and methodologies used to measure and report pick and place machine accuracy as a relationship to placement speed for a range of SMT component sizes and configurations. Purchase of this standard includes support documentation, report forms and the test material drawings in DWG format.
Document #:
Revision
C
Product Type
Released:  11/02/2017
Language
English
Current Revision
The IPC-J-STD-006C-AM1 amendment provides better detail of a solder alloy's maximum allowed deviation about the nominal level of the element's mass than was provided in past alloy standards. The IPC-J-STD-006C-AM1 amendment provided information on negative effects of adding rare earth elements to specific, heavy tin-containing, lead-free solder alloys and propensity of tin whisker formation...