IPC-J-STD-002E prescribes test methods, defect definitions, acceptance criteria, and illustrations for assessing the solderability of electronic component leads, terminations, solid wires, stranded wires, lugs, and tabs. The IPC-J-STD-002E standard also includes a test method for the resistance to dissolution/dewetting of metallization. IPC-J-STD-002E is intended for use by both supplier and user...
This standard prescribes test methods, defect definitions, acceptance criteria, and illustrations for assessing the solderability of electronic component leads, terminations, solid wires, stranded wires, lugs and tabs. A test method for the resistance to dissolution/dewetting of metallization is also included in the standard. Intended for use by both vendors and users, J-STD-002D was developed by...
本标准规定了用于评估电子元器件引线、焊端、实芯导线、多股导线、焊片和接触片可焊性的测试方法、缺陷定义及验收标准,并附有相关图表。IPC-J-STD-002E还包括金属层耐溶蚀性/退润湿的测试方法。IPC-J-STD-002E适用于供应商和用户。J-STD-002E由EIA、IPC和JEDEC开发。
IPC-J-STD-002Eは、電子部品のリード、ターミネーション、単線、より線、ラグ、およびタブのはんだ付性を評価するための試験方法、欠陥の定義、許容基準を規定し、またイラストを示すものである。また、IPC-J-STD-002Eの規格には、はんだ食われ/はんだはじきに対する耐性の試験方法も含まれている。IPC-J-STD-002Eはサプライヤーおよびユーザーの両者による使用を目的としている。IPC-J-STD-002Eの規格は次の三つの組織によって開発された:ECIA、IPC、JEDEC。 65ページ。発行 2017年11月。
Coming Soon
IPC-7095E: Design and Assembly Process Implementation for Ball Grid Arrays (BGAs)
IPC-7530B: Guidelines for Temperature Profiling for Mass Soldering Processes (Reflow & Wave)
IPC-2294: Design Standard for Printed Electronics on Rigid Substrates
IPC-6904: Qualification and Performance Specifications for Printed Electronics on Rigid Substrates
IPC-4105: Specification for Metal Base Copper Clad laminates for Rigid Printed Boards