This standard establishes the classification system, the qualification and quality performance requirements for flexible metal-clad dielectric materials to be used for the fabrication of flexible printed circuitry and flexible flat cable. It encompasses 12 specification sheets that result from the combinations of various copper foil claddings; a polymer base dielectric selected from at least two...