Close

IPC-4204 Standard Only

Language

Products

Document #:
Revision
B
Product Type
Released:  09/05/2018
Language
English
Current Revision
IPC-4204B establishes the classification system, the qualification and quality performance requirements for flexible metal-clad dielectric materials to be used for the fabrication of flexible printed boards. It encompasses 12 specification sheets that result from the combinations of various copper foil claddings; a polymer base dielectric selected from polyesters, polyimides, liquid crystal...