IPC-4204B establishes the classification system, the qualification and quality performance requirements for flexible metal-clad dielectric materials to be used for the fabrication of flexible printed boards. It encompasses 12 specification sheets that result from the combinations of various copper foil claddings; a polymer base dielectric selected from polyesters, polyimides, liquid crystal...