IPC-4556 Amendment

Products

Document #:
Revision
Original Version
Product Type
Released:  01/01/2016
Language
English
The Amendment 1 to IPC-4556 made the following changes to the base specification: a) It added the absolute value of the maximum thickness for the immersion gold of 0.070 μm [2.8 μin] that accompanies the statistically valid minimum immersion gold thickness; b) It added two more photomicrograph images to provide better information on identifying nickel hyper corrosion; c) It added the basis of...