IPC-4921A: Requirements for Printed Electronics Base Materials (Substrates)

Member: $51.00

Nonmember: $102.00

This standard provides and defines key characteristics and test methods for procuring printed electronics substrates. Includes six materials specification sheets.

Number of Pages: 48
ISBN: 978-1-61193-308-6
Product ID: 4921-STD-0-P-0-EN-A