IPC-8921: 集成导电纤维、导电纱和/或导电线的机织型和针织型电子织物(E-Textiles) 的要求[
IPC-8921标准提供并定义了工业测试方法和指南,以提供与导电纤维、导电纱和/或导线相结合的机织和针织型电子织物的关键特性和耐久性的性能数据。 IPC-8921标准还提供了机织和针织电子纺织品、纤维、纱线和电线的经典说明,并包括20个新的电子纺织品术语和定义。
Single-Device DRM-Protected Document
This document has single-device/user digital rights management (DRM) protection. This document will only be accessible by a single user on a single device. If you are purchasing this DRM-protected document for another user, you will need to provide contact information for that user when placing your order.