J-STD-001F-WAM1: J-STD-001 Revision F with Amendment 1: Requirements for Soldered Electrical and Electronic Assemblies
J-STD-001F with Amendment 1 incorporates the requirements of J-STD-001F and J-STD-001F Amendment 1 into one document. Criteria are presented in a seamless J-STD-001 format, and there are no redline marks.
This document is the equivalent to using J-STD-001F and J-STD-001F Amendment 1. IPC brings this version to industry to minimize confusion for those using both documents and those wishing to update their documentation with the latest available format.