This is the Chinese Language version of J-STD-002C.This standard prescribes test methods, defect definitions, acceptance criteria and illustrations for assessing the solderability of electronic component leads, terminations, solid wires, stranded wires, lugs and tabs. This standard addresses both visual acceptance and force measurement solderability criteria for both tin-lead as well as lead-free...