Amendment 1 to IPC-4202A modifies the standard by correcting editorial errors; converts metric dimensional units of measure to those commonly used throughout industry; describes the flammability method of test and requirements for very thin materials (VTM); and corrects property requirement errors in all nine specification sheets contained in this standard.
Document #:
Revision
A
Product Type
Released:  03/01/2014
Language
English
Amendment 2 to IPC-4202A modifies the standard by changing only one requirement in property 9. ‘Propogation Tear Strength, minimum’ for a base dielectric thickness that ranges from ≤ 50 µm to < 102 µm; changing the propogation tear strength to 13.5 grams [0.476 ounces].