Product Details
IPC-4562A standard covers metal unsupported foils and foils supported by carrier films suitable for subsequent use in printed boards. IPC-4562B addresses the requirements of metal foils used in printed wiring applications.
Published Date
ISBN
978-1-63816-169-1
Pages
47
DoD Adopted
No
ANSI Approved
No