The IPC-7801A standard provides requirements for process control of conveyorized solder reflow ovens. It includes a methodology for performing temperature measurements over time to establish a baseline profile, and then provides requirements to verify repeatability through periodic verification of the oven profile.

IPC-7801 - Standard Only

Reflow Oven Process Control Standard

Document #:
Revision
Original Version
Product Type
Released:  04/14/2015
Language
English
IPC-7801 provides process control for solder reflow ovens by baseline and periodic verifications of oven profiles using a standard methodology to demonstrate acceptable oven performance repeatability. Equipment calibration and maintenance guidelines are provided. This standard is intended to verify the operating parameters of the reflow oven. This standard is not intended for the assembly product...
Document #:
Revision
Original Version
Product Type
Released:  09/14/2022
Language
Japanese
Current Revision
本書、IPC-7801は、標準的な手法を用いながら、オーブンプロファイルの基礎的かつ定期的な検証によるはんだリフローオーブンの工程管理を規定するものである。また、機器の校正と保守に関するガイドラインを提供されている。本規格は、リフローオーブンの動作上のパラメータを検証することを意図するものである。本規格は、組立品の製品プロファイル/レシピについて記述するものではない。本規格では、ベーパーフェーズ工程に関するガイダンスは記載していない。18ページ。2015年発行。翻訳年

IPC-7801 - Standard Only

再流焊炉工艺控制标准

Document #:
Revision
Original Version
Product Type
Released:  02/22/2018
Language
Chinese
Current Revision
描述 中文描述 IPC-7801为焊料再流焊炉提供了工艺控制,通过基线和采用一个标准方法获得曲线的周期性验来证明可接受的重复性能,提供了设备的校准和维护指南,本标准的目的是验证再流焊炉的运行参数,不适用于组装产品的温度曲线和工艺参数。 本标准不提供气相工艺的指导。全文18页。于2015年正式发布。2017年8月翻译。