IPC-8971 - Standard Only
Requirements for Electrical Testing of Printed Electronics E-Textiles
IPC-8971 is intended to assist in selecting the test equipment, test parameters, test data and fixturing required to perform electrical test(s) on printed electronics on e-textiles. Printed electronics on e-textiles is printed electronics on coated or treated textile substrates. Coatings and treatments may be applied for printability of the textile substrate and/or for performance of the textile substrate or finished printed electronics e-textile (e.g., hydrophobic, water retardance, flame retardance, surface energy). Coatings or treatments may be applied using printing, lamination or other processes.