Surface mount pad cratering typically initiates prior to detection by existing electrical monitoring test methods. There are limited instrumentation techniques that are currently available that can identify non-electrical damage and its location to a high degree of accuracy. This guideline document establishes an acoustic emission (AE) method to evaluate the performance and reliability of surface...