Current Revision
The IPC-J-STD-006C-AM1 amendment provides better detail of a solder alloy's maximum allowed deviation about the nominal level of the element's mass than was provided in past alloy standards. The IPC-J-STD-006C-AM1 amendment provided information on negative effects of adding rare earth elements to specific, heavy tin-containing, lead-free solder alloys and propensity of tin whisker formation...
Document #:
Revision
B
Product Type
Released:  09/01/2009
Language
English
Amendments 1 & 2 to IPC J-STD-006B make the following nine changes to the basic document: 1. Correct some editorial mistakes in the document's text, 2. Add reference to IPC/JEDEC J-STD-609, Lead-Free and Leaded Marking, Symbols and Labels, 3. Clarify the meaning of those alloys that are designated as lead-free, 4. Provide guidance to suppliers how to designate and mark lead-free alloys, 5. Correct...