Evaluation of Steam Aging on Alternative Finishes, Phase 11A
Details the results of a two-year study to determine the effect of steam aging exposure on components. A variety of solderable finishes were used. A small production simulation utilized preconditioned and as-received samples and tested a total of 2,000 joints. 15 pages. Released July 1996.