This technical report provides the documentation of a round robin testing effort that generated data used by the 4-14 Plating Processes Subcommittee in developing the maximum immersion silver plating thickness requirement in the revision A of IPC-4553. This compendium of data resulted from three information sets: a) Test vehicle assembly report by Celestica, b) Thermal cycle test report by...