This standard addresses semiconductor flip chip design requirements. Provides information for using standard semiconductor substrates, materials, assembly and test methods with established fabrication, bumping, test and handling practices. Electrical, thermal and mechanical chip design parameters and methodologies are covered in the standard, as well as the reliability aspects associated with...