Close

IPC/JEDEC-9704 Standard Only

Your results

  • 1

Language

Products

IPC-9704 - Revision A - Standard Only

Printed Circuit Assembly Strain Gage Test Guideline

Document #:
Revision
A
Product Type
Released:  02/03/2012
Language
English
Current Revision
Strain gage testing allows for objective analysis of the strain and strain rate levels to which a surface mount package may be subjected to during assembly, test and operation. Excessive strain can result in various failure modes for different solder alloys, package types, surface finishes or laminate materials. This document describes specific guidelines for strain gage testing during the printed...