Products
This standard on spherical transient bend testing is intended to characterize the maximum allowable strain that a surface mount component's board level interconnects can withstand in flexural loading. Whereas four-point monotonic bend test methods only address simple planar bending, spherical bend tests establish strain limits of board level interconnects under worst-case flexure conditions that...
Coming Soon
IPC-7095E: Design and Assembly Process Implementation for Ball Grid Arrays (BGAs)
IPC-2294: Design Standard for Printed Electronics on Rigid Substrates
IPC-6904: Qualification and Performance Specifications for Printed Electronics on Rigid Substrates
J-STD-005B: Requirements for Soldering Pastes
IPC-4105: Specification for Metal Base Copper Clad laminates for Rigid Printed Boards
J-STD-004D: Requirements for Soldering Fluxes
IPC-4413: Specification for Finished Fabric Woven from Low Dk Glass for Printed Boards