IPC/JEDEC-J-STD-035 - Standard Only
Acoustic Microscopy for Non-Hermetic Encapsulated Electronic Components
This test method defines the procedures for performing acoustic microscopy on non-hermetic encapsulated electronic components. It provides users with an acoustic microscopy process flow for detecting defects non-destructively in plastic packages while achieving reproducibility. Developed by IPC and JEDEC. 16 pages. Released April 1999.
Equivalent to IEC Publicly Available Specification (PAS) 62191