This document provides tests that record changes in surface insulation resistance (SIR) on a representative sample of a printed circuit assembly. It quantifies any deleterious effects that might arise from solder flux or other process residues left on external surfaces after soldering, which can cause unwanted electrochemical reactions that grossly affect reliability. It uses test vehicles that...