J-STD-003C prescribes test methods, defect definitions and illustrations for assessing the solderability of printed board surface conductors, attachment lands, and plated-through holes utilizing either tin-lead or lead-free solders. This standard is intended for use by both vendor and user. The objective of the solderability test methods described in this standard is to determine the ability of...