Guidance to reduce and control exposure to environmental conditions and contamination that promote the development of White Plague is provided in this document. A template for developing a White Plague Control Plan (WPCP) is included.
Guidance to reduce and control exposure to environmental conditions and contamination that promote the development of Red Plague is provided in this document. A template for developing a Red Plague Control Plan (RPCP) is included.