The IPC-J-STD-006C-AM1 amendment provides better detail of a solder alloy's maximum allowed deviation about the nominal level of the element's mass than was provided in past alloy standards. The IPC-J-STD-006C-AM1 amendment provided information on negative effects of adding rare earth elements to specific, heavy tin-containing, lead-free solder alloys and propensity of tin whisker formation...

IPC-J-STD-001 - Revision F - Amendment 1

Cerințe pentru Ansamblurile Electrice și Electronice Lipite

Document #:
Revision
F
Product Type
Released:  11/28/2016
Language
Romanian
Current Revision
Acesta este un amendament la standardul IPC J-STD-001F, un standard industrial recunoscut și adoptat, acoperind cerințe de materiale și procese. Modificările includ, fără a se limita la acestea, o revizuire a cerințelor minime de umplere cu aliaj a găurilor metalizate, PTH, o schimbare a criteriilor pentru goluri la circuitele BGA cu bile fără turtire, reprezentări grafice noi pentru montarea...