IPC-4556-AM1 is the amendment 1 to the standard IPC-4556 and made the following changes to the base specification: a) It added the absolute value of the maximum thickness for the immersion gold of 0.070 μm [2.8 μin] that accompanies the statistically valid minimum immersion gold thickness; b) It added two more photomicrograph images to provide better information on identifying nickel hyper...
Document #:
Revision
Original Version
Product Type
Released:  09/01/2013
Language
English
Current Revision
IPC-4554, "Specification for Immersion Tin Plating for Printed Circuit Boards," is the third document in a series of specifications [the first two are: IPC-4552 which addresses electroless nickel/immersion gold (ENIG) and IPC-4553 which addresses immersion silver (IAg)] that set the requirements for printed circuit board surface finishes that are alternates to eutectic tin-lead. IPC-4554, a full...