Ergänzung 1 zu IPC-7711/21C-DE, das Dokument enthält Verfahren für das Entfernen und Montieren von D-Pak-Komponenten.
Enmienda 1 al IPC-7711/21C, el documento proporciona los procedimientos para la extracción y la instalación de componentes D-Pak.
The Amendment 1 to IPC-4556 made the following changes to the base specification: a) It added the absolute value of the maximum thickness for the immersion gold of 0.070 μm [2.8 μin] that accompanies the statistically valid minimum immersion gold thickness; b) It added two more photomicrograph images to provide better information on identifying nickel hyper corrosion; c) It added the basis of...
Specification for Electroless Nickel/Immersion Gold (ENIG) Plating for Printed Circuit Boards Amendment 1 to IPC-4552 replaces the Table 3-1 Requirements of Electroless Nickel Immersion Gold Plating plus also replaces all of sections 3.2.1 Immersion Nickel Thickness and 3.2.2 Immersion Gold Thickness in the original release of the IPC-4552. The Amendment 1 permits the use of thinner gold (≥4 µm...
Specification for Electroless Nickel/Immersion Gold (ENIG) Plating for Printed Circuit Boards Amendment 2 to IPC-4552 is a new section in the original release of the IPC-4552. The Amendment 2 provides the “rules” by which any rework and/or repair of a printed board's ENIG surface finish is allowed. Effective September 2012.
The amendment 2 to IPC-9121 provides new troubleshooting topics on hole quality, laser drilling, microvias, drill smear, electroless nickel, organic solderability preservative (OSP) and rigid-flex boards.
IPC-9121 AM1 is an amendment to IPC-9121 which provides updates to the Hole Preparation/Protection and Interconnect Formation sections, covering troubleshooting topics and guidance on nonconductive plugging paste, microvias and pattern plating rim voids. IPC-9121 AM1 also includes a new section on Flexible Circuits.
The IPC-1791-Am1 provides revisions and clarifications for requirements pertaining to CAGE Code, citizenship, security, foreign person access, traceability records and NIST SP 800-171 compliance.
The Amendment 2 to IPC-4103A-WAM1 made four fundamental changes to the base standard: All references to the epoxy curative of DICY (dicyandiamide) were removed; Opaque foreign inclusions were more specifically defined and limited; The optional properties of thermal conductivity for both laminates and bonding layers were added; and The dielectric constant (permittivity) ranges were specifically...
本手册可供任何生产制造或采购印制板的人员作为基本资源。数百张真实的全彩色照片聚焦了650多个印刷电路板工艺缺陷,每个缺陷都有其分析原因和纠正措施。IPC-9121是取代1997年12月发布 的IPC-PE-740A中的PCB部分。2016年3月发布9121英文母标准,2018年年4月发布修订本1,修订本1于2020年4月翻译。详情参见目录。
Coming Soon
IPC-7095E: Design and Assembly Process Implementation for Ball Grid Arrays (BGAs)
IPC-7530B: Guidelines for Temperature Profiling for Mass Soldering Processes (Reflow & Wave)
IPC-2294: Design Standard for Printed Electronics on Rigid Substrates
IPC-6904: Qualification and Performance Specifications for Printed Electronics on Rigid Substrates
IPC-4105: Specification for Metal Base Copper Clad laminates for Rigid Printed Boards