This standard is intended as a guideline in the proper preparation of a metallographic sample (microsection) of a printed board. The finished microsection is used for evaluating the quality of the laminate system and plated structures (e.g. PTHs and vias). Microsection sample preparation is regarded by many as a highly developed skill. The guidelines in this standard discuss the many variables and...
Mechanical bend and shock tests are routinely performed on SMT assemblies to ensure that they can sustain anticipated production, handling and end use conditions. The strains and strain rates applied to SMT assemblies during bend and shock testing can lead to a variety of failure modes in the vicinity of the solder joints. This document provides test methods to evaluate the susceptibility of...
Provides information on design characteristics and the application of solderless surface mount connectors, including conductive adhesives to aid IC package and board interconnection. 34 pages. Released January 1994.
Establishes the requirements for the evaluation of liquid and dry film solder mask material and for the determination of the acceptability of use on a standard printed board system. IPC-SM-840 provides two classes of requirements, T and H, to reflect functional performance requirements and testing severity based on industry/end use requirements. Coverage is given to adhesion, material qualification...
This publication is intended to characterize the frature strength of a component's board level-interconnect by providing a common method of establishing the fracture resistance to flexural loading that may occur during conventional non-cyclic board assembly and test operations. The document is applicable to surface mount components attached to printed wiring boards using conventional solder reflow...
Survey-based study presents data and analysis on the EMS industry, examining trends in sources of revenue, revenue per employee, services offered, markets served, manufacturing technology, capital investment, spending on equipment and materials and market size including forecasts and potential for market expansion. This study is based on data provided by a representative sample of 120 EMS...
Every electronics manufacturer, whether an original equipment manufacturer (OEM) or electronics manufacturing services (EMS) company, must determine if the unpopulated printed boards entering the assembly process have an adequate level of cleanliness. The question of “how clean is clean enough?” is one that has no definitive answer, as there is no "golden number" for board cleanliness. The issue...
Provides specific test methods to evaluate the performance and reliability of surface mount solder attachments of electronic assemblies. Establishes levels of performance and reliability of the solder attachments of surface mount devices to rigid, flexible and rigid-flex circuit structures. When used with IPC-SM-785, it provides an understanding of the physics of SMT solder joint failure and an...
This is the industry standard for qualification and quality conformance of conformal coating. Its intent is to show how to obtain maximum information with minimum test redundancy. Includes requirements and evaluations of material properties using standardized test vehicles. Amendment 1 updates include new qualification, retention and conformance inspection requirements for FTIR, MIR and hydrolytic...
Ce document essentiel pour l’industrie fournit des descriptions et des illustrations de la terminologie de l’industrie d’assemblage électronique afin d’aider les utilisateurs et leur clients à casser les barrières linguistiques. La révision M contient plus de 220 termes nouveaux ou révisés, incluant la nouvelle terminologie pour les procédés de tropicalisation, d’enrobage et d’encapsulation, la...
Implementing Ball Grid Array (BGA) and Fine-Pitch Ball Grid Array (FBGA) technology presents some unique challenges for design, assembly, inspection and repair personnel. IPC-7095B delivers useful and practical information to anyone currently using BGAs or considering a conversion to area array packaging formats. This has become especially important due to the change in the alloys being used, both...
Implementing Ball Grid Array (BGA) and Fine-Pitch Ball Grid Array (FBGA) technology presents some unique challenges for design, assembly, inspection and repair personnel. Revision A of this document delivers useful and practical information to anyone who is currently using BGAs or is considering a conversion to area array packaging formats. In addition to providing guidelines for BGA inspection...
IPC-T-50N-CN文件旨在为电子行业中常用的词汇和术语提供其定义。本文件所规定的定义充分详细地阐明了术语,以便以英语为第二语言的读者能够理解含义的细微之处。IPC-T-50N-CN包含550多个新的或修订的术语,包括通孔结构、表面贴装器件类型、焊料凸点、焊料合金、焊接、退润湿、电路板制造工艺和测试的新术语。
Das unentbehrliche Nachschlagewerk für alle Verantwortlichen entlang der Wertschöpfungskette von elektronischen Produkten. Die Revision K enthält auf mehr als 120 Seiten, mehr als 220 neue und überarbeitete Begriffe und bildliche Darstellungen. Beispiele: Access Hole, Accelerated Equivalent Soak, Capture Land, Micro Via Technology, Plating Thief, Etchback, Resin Recession, Tape Automated Bonding...
IPC-CC-830B prescribes qualification and performance requirements of conformal coatings. Amendment 1 provides updated requirements for moisture and insulation resistance and temperature and humidity aging and additional information on coating classifications.
IPC-7095D在设计,组装,检查和维修过程中实施球栅阵列(BGA)和细节距球栅阵列(FBGA)技术提出了了一些独特的挑战。它为使用或正在考虑使用BGA的用户提供有用和实用的信息。 它还介绍了如何使用BGA成功实现印刷电路板组件的稳健设计和装配流程,以及解决BGA组装过程中可能出现的一些常见异常的方法。由于焊球中合金,焊球形状,封装程序等的改变,许多问题变得尤为重要。D版主要重点是为组装后出现的一些新的机械失效问题如坑裂或层压缺陷提供信息。除了提供BGA检查和维修的指引外,本标准还解决了与BGA相关的可靠性问题和无铅焊点的使用标准。该标准中有许多X射线和内窥镜的照片和插图以确认行业中BGA组装工艺的实施中的遇到的一些情况。
IPC-7095D-AM1は、ボールグリッドアレイ(BGA)およびファインピッチBGA(FBGA)技術の設計および組立の実施について記述するものであり、これらのパッケージを使用したプリント基板の設計と組立に関連する検査、リペアおよび信頼性の問題に焦点を当てている。 IPC-7095D-AM1は、BGAを使用している、もしくは使用を検討している本書読者に対し、有用で実用的な情報を提供するものである。またIPC-7095D-AM1では、BGAを使用するプリント基板組立のためのロバスト設計と組立プロセスの正しい方法について説明するとともに、BGAの組立中に発生する可能性のある一般的な異常について、トラブルシューティングの方法を説明している。
简要介绍 (英文) 建立了液态和干膜阻焊材料的评估要求,以及确定其用在一个标准的印制板系统上的可接受性要求。IPC-SM-840提供了两个等级的要求,T级和H级,以反映基于行业/最终用户要求对功能性的要求及测试严格程度的差别。覆盖了附着力、材料鉴定、耐溶剂、以及电气要求。E版本包含了挠性覆盖材料的要求,在已蚀刻的导体和其他导电图形上提供挠性的介质保护层。共19页。2010年12月发布。2012年10月翻
本文件是IPC电化学迁移(ECM)技术组的成果。本文件的目的是为如何更好地使用IPC-TM-650测试方法2.6.25《耐导电阳极丝(CAF)测试》以及其他内部电化学迁移(ECM)测试提供指南,以评估机械应力、层压板材料断裂、离子污染、压合层压板前湿气含量以及其它材料加工特性在层压材料中形成的导电路径,例如导电阳极丝(CAF),一种特殊类型的ECM失效模式,对测试结果的影响。该内部ECM测试方法提供了一个已经证实的标准,用于确定由于通孔偏移从而显著降低内部导体间绝缘电阻情况的风险,该现象发生在层压板内部,而不是在印制板的表面上
材料の適合性を検証するにあたり、業界では種々のテストビークルが存在し活用されている。IPC-B-52試験基板は実生産で用いられる材料と工程を具体的に表現したものであり、イオンクロマトグラフと表面絶縁抵抗(SIR)の両試験のニーズを満たすテストビークルである。IPC-9203Aに示す規格はIPC-B-52テストビークルに対応し、製造工程の評価や、選択した製造材料セットと工程が清浄度の観点から適合しているという客観的証拠を提供する場合に利用できる。またIPC-9203Aに示すユーザーガイドラインはIPC-9202の手引き文書として作成されており、製造者が材料と工程の適合性を実証する場合の規定「~することが望ましい」と「~すること(する必要がある)」という点について明確に提示している。
概説 本書、IPC-9202A「材料・工程の特性評価/認定試験の方法」は、プリント回路組立品(PCA)の代表的なサンプル上の表面絶縁抵抗(SIR)の変化を記録するものである。この試験は、はんだ付後に外層に残るはんだ由来のフラックスまたはその他の工程残さが原因で不要な電気化学的反応を引き起こし、信頼性に重大な影響を及ぼす可能性について定量化するものである。 この試験では、実際の生産工程において電子回路の代表的なものとなるような基板をテストビークルとして使用する。これは、定量的かつ定性的なデータの両方を得ることができる試験である。 IPC-9202Aに紹介する試験は、提案された製造工程や工程変更を用いた場合に、生産するハードウェア(製品)の最終的な性能が電気化学的リスクに対し許容可能であるということを示すための「工程認定」用として使用することができる。工程変更には組立工程の手順...
規格「IPC-CC-830C」は、電気絶縁化合物 (コンフォーマルコーティング) の認定および適合要件について確立するものである。これは、最小限の冗長テストで材料の最大の信頼性を得ることを目的として、設計および構築されてきたものである。規格「IPC-CC-830C」は次の項目を対象とする: フォーマルコーティング剤の認定および認定の維持 (表3-1、コラムAおよびB)。 コンフォーマルコーティング剤の特性に関する品質適合性 (表3-1、コラムC)。 本規格においてコンフォーマルコーティングという用語は、プリント配線板組立に使用される保護コーティングのタイプを指す場合に用いられる。コンフォーマルコーティングは単に機械的な支持をもたらすものではなく、湿気および汚染から基板を保護し、電気絶縁を付与することを目的としている。
本标准规定了电气绝缘化合物(敷形涂覆材料)的鉴定和符合性要求,并设计和构建了充分且必要的测试项目来获取对材料性能的信心。本标准包括: 敷形涂覆材料的鉴定及鉴定效力保持(表3-1,A 列及B 列)。 敷形涂覆材料属性的质量符合性(表3-1,C 列)。 本标准中,敷形涂覆是指用于印制线路组件的保护涂层。敷形涂覆可起到防潮、防污物和电气绝缘的作用,但不是作为单独起机械保护作用的涂层。
Coming Soon
IPC-7095E: Design and Assembly Process Implementation for Ball Grid Arrays (BGAs)
IPC-7530B: Guidelines for Temperature Profiling for Mass Soldering Processes (Reflow & Wave)
IPC-2294: Design Standard for Printed Electronics on Rigid Substrates
IPC-6904: Qualification and Performance Specifications for Printed Electronics on Rigid Substrates
IPC-4105: Specification for Metal Base Copper Clad laminates for Rigid Printed Boards