The IPC-WP-116A white paper provides guidance to control and mitigate risks associated with the introduction of Foreign Object Debris (FOD) in electrical and electronic assemblies. Guidance to control and mitigate risks associated with the introduction of Foreign Object Debris (FOD) in electrical and electronic assemblies is provided. A template for developing a Foreign Object Debris (FOD) Control...

IPC-WP-001 - White Paper

Soldering Capability White Paper Report

Document #:
Revision
Original Version
Product Type
Released:  08/01/1991
Language
English
Current Revision
Due to a concern in the electronic packaging industry about solderability problems, Foster Gray, PC Interconnects, developed this document for the Surface Mount Council. Areas covered are: design for the soldering process; solderable PWBs; solderable components and soldering process. Five different industry perspectives provide analysis of these issues. 35 pages. Released August 1991.
Document #:
Revision
Original Version
Product Type
Released:  05/01/2018
Language
English
Current Revision
IPC-WP-023 is an IPC Technology Solutions White Paper addressing reliability issues associated with stacked microvias. There is evidence that staggering vias can result in a more robust structure; however, staggering microvias is only a temporary solution to accommodate complex designs with microvias built with weak interface structures IPC-WP-023 white paper provides an investigation of these...
Document #:
Revision
Original Version
Product Type
Released:  12/05/2019
Language
English
Current Revision
The IPC-WP-026 white paper explores blockchain as an emerging technology that has a core strength in providing an immutable, auditable, transparent and secure environment for data exchanges. These advantages make it a prime candidate for implementation in the electronics industry. The IPC-WP-026 white paper explores blockchain and its limitations and challenges. It also provides a few directions...
Document #:
Revision
Original Version
Product Type
Released:  08/16/2018
Language
English
Current Revision
IPC-WP-024 is a white paper which discusses the issues associated with reliability of smart textiles (e-textiles structures) following multiple washing cycles and emphasizes efforts that industry and research laboratories must undertake to make e-textile structures more robust and able to be washed similarly to everyday textile products (e.g., underwear, clothing, home textiles and technical...
Document #:
Revision
Original Version
Product Type
Released:  04/01/2019
Language
English
Current Revision
This white paper is a benchmarking exercise of e-textile integrations, providing an introductory categorization of how the current market sector is using textile-based electrical components to achieve integrated functionality. This peer assessment provides a baseline understanding of e-textile process techniques, requirements and resources within this emerging sector.
Document #:
Revision
Original Version
Product Type
Released:  09/05/2018
Language
English
Current Revision
Manufacturers of high reliability electronics have been working for many years to mitigate the deleterious effects of tin whisker formation. One highly effective means to suppress the growth of tin whiskers is to replace the pure tin plating with reflowed tin-lead solder. One approach is to fully consume the tin plating by tin-lead solder during the SMT reflow process. This phenomenon of tin...

IPC-WP-004 - White Paper

Design for Success

Document #:
Revision
Original Version
Product Type
Released:  08/01/1994
Language
English
Current Revision
Addresses the complete process of reengineering new product development processes to incorporate DFX methodologies. Presents the case for a comprehensive analysis of the key business issues and definition of requirements before initiating work to refine or restructure processes. Editor, Dieter Bergman, IPC. 88 pages. Released by the Surface Mount Council, April 1997.

IPC-WP-003 - White Paper

Chip Mounting Technology

Document #:
Revision
Original Version
Product Type
Released:  08/01/1993
Language
English
Current Revision
Status of the technology discussion on the various methodologies for mounting and interconnecting active devices to a variety of substrate materials is summarized in this document. Reviews mounting techniques of tape automated bonding (TAB), chip on board (COB) and flip chip. Examinations of the most commonly used substrate options of laminate, ceramic and silicon are also reviewed. Editor: John...

IPC-COMPTRACE-609 - White Paper

What You Can Do About Component Traceability

Document #:
Revision
Original Version
Product Type
Released:  07/07/2009
Language
English
Current Revision
The problem of counterfeit components continues to escalate. It is no longer limited to high value items like semiconductors. It can include connectors, resistors, passive components or anything that is in demand. What more could you be doing to ensure that the components you purchase are genuine? What can you do about component traceability? Jack Stradley, Manager, Business Development &...
Document #:
Revision
Original Version
Product Type
Released:  04/16/2019
Language
Chinese
Current Revision
IPC-WP-024是一份白皮书,讨论了多次洗涤循环后智能织物(电子织物结构)可靠性相关的问题,并强调了工业和研究实验室必须做出的努力。以使电子织物结构更加坚固,能够像市场上的日常织物(例如,内衣、服装、家用织物和技术织物)一样被清洁或洗涤。 研究人员在商用洗衣机和家用洗衣机洗涤剂多次洗涤循环后,为电子织物提供实验室测试的初始可靠性结论。