This technical report provides full detail of the round robin study charged with assessing the use of Interconnect Stress Test (IST) as a test for incoming inspection in lieu of Thermal Stress in the detection of innerlayer separations in plated-through holes. Includes background on the Post Separation Task Group, test results, round robin test plan, conclusions and test methods used. 51 pages...